TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 12 Jul 2011 03:59:26 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (149 lines)
Hi folks - Here is the Friday Element Quiz Answer (sorry for the posting 
delay, was at a dragonboat festival this weekend):

The Question:

This element has no biological role and is never encountered outside 
nuclear facilities. The total world production of this element to date is 
estimated to less than a millionth of a gram. A piece of this element has 
never been seen by the naked eye as its intense radioactivity would 
immediately result in its complete evaporation. The total amount of this 
element found in the Earth's crust is estimated to be less than 30 grams. 
What element is being described?

The Answer:

The element is Astatine (At). Astatine is easy to produce by bombarding 
bismuth with high energy alpha particles but because it is so volatile and 
highly radioactive very little is known about it. Much of the data on 
Astatine is from the study of extremely dilute solutions or from its 
position in the Periodic Table. Astatine was discovered by D. Corson, K. 
Mackenzie and E. Segre in 1940 but due to the resource demands of the 
Manhattan Project, very little research was conducted on it. Astatine was 
finally named in 1947. In 1931, a group of chemists lead by F. Allison 
reported they had discovered the element below Iodine which they named 
Alabamine (after the state of Alabama in the US) but their claim could not 
be confirmed. 


The quiz winner is Nigel Burtt who will get the services of Clumpy and 
Kloumpios. The guys will fire up their John Deere tractors and make their 
way from Brian's house in Cyprus to Nigel's facility in the UK.

So far Clumpy and Kloumpios have:

Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)

Week 2 Bev Christian, RIM
- conducted REACH material testing

Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn

Week 4 Ian Fox, Goodrich
- had an epic journey of travel

Week 4 Gary Ferrari, Garrick Global
- unknown

Week 5 Fredrick Miller, Astrolab
- unknown

Week 6 David Nelson, Raytheon
- Were tackling dummys for Dallas Cowboys

Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim

Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown

Week 9 Steve Gregory of RD Circuits
- unknown

Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!

Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit

Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!

Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process

Week 14 Bev Christian, RIM
- assisted with a tin pest investigation/test

Week 15 Bev Christian, RIM
 - assisted Bev shoveling snow

Week 16 David Bealer of Watchfire Signs
 - assisted with reflow profiling

Week 17 Brian Ellis, rumored to be retired
 - assisted with rewiring the house, had a tractor accident and found his 
cousin Kloumpios

Week 18 Denny Fritz, SAIC
 - assisted with tin whisker inspection/examinations

Week 19 Graham Collins, L3 Communications
- assisted with scraping barnacles, boat paint and boat engine maintenance

Week 20 Mark Woolley, PTRL Laboratory Avaya
- assisted with weather observations (70F to snow) and resolving 
electrochemical migration failures

Week 20 Tom Carroll, Boeing Defense, Space and Security
- assisted with commercial aircraft galley inspection

Week 21 Brian Ellis, supposedly retired, and Tom Carroll, Boeing Defense, 
Space and Security
- assisted with root cause corrective action tasks
- assisted with nothing but catching up with the family

Week 22 Drew Meyer, Benchmark Electronics Inc.
- assisted with metallographic cross-sections and Dye & Pry testing

Week 23 Bev Christian, RIM
- assisted with a creep corrosion project and the setting up of an oxygen 
bomb

Week 24 Steve Gregory, RD Circuits
- unknown

Week 25 Ahne Oosterhof, A-Laser
- assisted with stencil aperture data analysis and split/stacked firewood

Week 26 Scott Post, Delphi
- assisted/participated in the Kokomo Airshow Race Event

Week 27 Brian Ellis, supposedly retired
- assisted with tedious website work and family home cooking

Week 28 Nigel Burtt, ???
- assisted with ???


Dave Hillman
Rockwell Collins
[log in to unmask]

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2