Hi Earl,
I donīt think itīs any good what you have in mind with your fine pitch
parts. If you have them in a tray better leave them there, supply only trays
to your line, handle them according their moisture level, reseal the bags
and send the remaining parts back to your stock.
For safe repacking you will need to have some kind of equipment, a
manipulator seems to be the minimum requirement for that task, all necessary
ESD measures and operators with enough sensitiveness to handle those
delicate parts, all things that normally arenīt found in stockrooms.
Donīt get yourself in trouble
Wolfgang
-----Ursprüngliche Nachricht-----
Von: Wildes, Earl [mailto:[log in to unmask]]
Gesendet am: Freitag, 16. November 2001 16:53
An: [log in to unmask]
Betreff: [TN] handling single parts
Hi there. I sent this out once before, but it might have bounced.
Is there any guideline or procedure detailing how to handle single surface
mount parts, especially fine pitch. I've found several on moisture and ESD,
but none on re-packaging. Our production numbers are rather low, so it is
not always best to issue the whole tray of parts to the board shop. We need
a document to teach the stockroom personnel how to pick up and package
individual parts without bending the leads.
Thanks for your help.
Earl Wildes
Sr. Component Engineer
Korry Electronics Co.
901 Dexter Ave N.
Seattle, WA 98109
206-694-1398
[log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|