TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, karpinski <[log in to unmask]>
Date:
Tue, 17 Feb 2004 16:21:42 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
Hi Waclaw,

Do you know what material (Pd or Ru) your board supplier uses to deposit electroless Ni?

Vladimir Igoshev, 
Research in Motion

Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask] <mailto:[log in to unmask]> 


-----Original Message-----
From: karpinski [mailto:[log in to unmask]]
Sent: Wednesday, February 18, 2004 4:15 PM
To: [log in to unmask]
Subject: [TN] Ni/Au solderability on kapton


Recently we have solderability problems with Ni/Au kapton flex boards
(0,1 µm Au, 3 µm Ni, 35m Cu).
We have produced and assembled large number of boards.
On 10 % of the boards we observe interconnection failures after final
assembly of the pcbs. If  the suspected solder joints are lightly
stressed , the connections are easily broken, leaving an open circuits.
 It is  easy to peel  these parts with solder material  from the boards.
The pads below the removed parts are discolored dark gray and are sleek .
Some times the handsoldering of the broken joins was successful but
after small strain the joints  broke again.
Additional vapor phase soldering  did not improved the the strength of
the joints.
This is new problem for us. Does anyone have any experience with this?
How to rework the boards? How to determine when a board should be
reworked or
scrapped? What about reliability issues? Latent failures?
I would appreciate your help very much
  regards

--
Waclaw Karpinski
I. Physikalisches Institut
RWTH Aachen
D - 52074  Aachen

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2