Hello.
I'm looking for some clarification on TM 650 Number 2.6.3.3, Surface
Insulation Resistance, Fluxes.
I am testing no clean fluxes, thus using sample groups B, C, and F (ie
patten down/no clean, pattern up/no clean and control groups).
Looking at the document, I interpret it to mean that I require 6 coupons (3
for each of B and C) for each condition I'm testing, as well as 2 control
coupons.
This amounts to, say, 26 coupons (104 combs) to test 4 conditions.
Does this number sound right, or much too high? Is the industry norm to
follow the standard to the letter, or to use a reduced number of samples?
Or do I simply need to test 6 combs, 3 per pattern up and down (per
condition)?
Thanks in advance for any advice:-)
Cara Startek
Process Engineering
http://www.leitch.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|