Kevin Glidden <[log in to unmask]>
Reply To:
Date:
Mon, 17 Oct 2005 11:43:10 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (53 lines)
Appendix A of J-STD-001D lists conditions and dispositions by class (eg:
Acceptable Class 1, Process Indicator Class 2, Defect Class 3)


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Seymour
Sent: Friday, October 14, 2005 1:57 PM
To: [log in to unmask]
Subject: [TN] Class 2 Vs 3

Happy Friday,

Does anyone know of a good source for a spreadsheet or matrix comparing
Class 2 to Class 3 for fabrication and assembly?

Thanks
Dave

--
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560

Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297

[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2