Steve
Use the Paralene, because the solvents in the PU will likely not improve the dry-film
mask, either.
Brian
"Stephen R. Gregory" wrote:
> Hi ya'll...
>
> Well I've run into a problem again that I've experienced a few times before.
> I've got a board (actually 3 boards) here, where the solder mask has come off
> all the surface traces. I know what's caused it, it's because of a certain
> brand dry-film mask is not compatible with the brand of cleaning chemistry
> that we use, the mask starts flaking off if it's washed more than twice I
> don't want to mention names because I upset some people last time when I
> did...
>
> The problem is how can I go about repairing the boards. It's a small
> double-sided board with some very long lead time PTH resistors on it and
> 2-connectors, and as I said, it's only 3-boards.
>
> The board is hi-rel, and these 3 boards are needed to complete a system. The
> board gets conformal coated as a normal part of the process. We spray a
> 2-part urethane here, but at one of our other facilities we do have paralene
> vapor deposition capabilities.
>
> I know trying to touch-up the mask is out of the question because as I said,
> the mask has flaked-off of all the surface traces. Do any of you have a
> opinion as to whether the urethane would be sufficient, or should I use
> paralene? I tend to think that paralene would be better because of it's
> strength and ability to coat all surfaces well.
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|