Dear Jean-Francois,

Please feel free to contact me off line for any info regarding conformal
coating removal.  

Best Regards,

Phil Kinner
Chief Chemist

Concoat Ltd
Millfield House, 9-11 Fleet Road,
Fleet, Hants, GU51 3QF

Tel:- +44 1252 813706
Fax:-+44 1252 813709
Mob:- +44 7919 470958

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bissonnette,
Jean-Francois
Sent: 11 February 2003 14:11
To: [log in to unmask]
Subject: [TN] Conformal coating removal

I would like to contact someone offline concerning conformal coating
removal.
Coating types are various.

Anyone have that expertise???

Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1

(514) 335-4200 x2021
(514) 335-4231 fax



***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged
and confidential information intended only for the use of the individual
or entity named herein. If the reader of this transmission is not the
intended recipient, you are hereby notified that any dissemination,
distribution, or copying of this transmission is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2