All fluxes, by definition, must have some form of corrosive ion for it
to be able to reduce metal oxides. Even pure rosin isomers have a
carboxylic acid group. From your description, it seems probable that you
have what is effectively a short-circuited battery with gold and copper
as your electrodes with bare copper where the fingers are cut or the
gold plating is too thin/porous/worn through. Any condensation would
provide you with an electrolyte, exacerbated by tthe presence of any
ionogenic and/or hygroscopic contaminant (not necessarily from your
flux, which you don't want on gold-plated fingers, anyway).
Brian
On 29/02/2012 16:53, Victor Hernandez wrote:
> Fellow TechNetters;
>
> Do No Clean LF fluxes, Rosin Core/molten solder, have a corrosive ion? Every so often when conducting analysis on Field Return Product I notice small amount of corrosion product on gold plated contact on DIMM and PCI Slot connector. Sometimes on other gold plated connector leads. So I am trying to understand which component had a corrosive ion waiting for the right conditions to flourish. Small amount of greenish/bluish residue. It can be seen on wipe zone and/or stamp edge of contact. Where is this active corrosive ion coming from?
>
> Can someone provide the link to Stevezea home page for posting pictures?
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|