Content-Transfer-Encoding: |
7bit |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Fri, 5 Oct 2001 12:52:35 +0200 |
Content-Type: |
text/plain; charset="iso-8859-1" |
MIME-Version: |
1.0 |
Reply-To: |
|
Parts/Attachments: |
|
|
Hello all,
Maybe this is a strange question but there are very much absoletb components
to be placed on the boards.
I like to know if there is a test method on testing MLB boards for
delamination.
I have been thincking about placing the boards into a oven for a while
before soldering the boards. What time should i use in the oven and at what
temperature to be sure there will be no delamination.
The soldermethode for these boards is 2 x reflow an 1 x wave.
Best regards,
Gerard Goossens
Flatfield multi print
Tel :+31-344-622556
Fax :+31-344 613652
-----------------------------------
Mail : [log in to unmask]
Website : www.flatfield.nl
-----------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|