text/plain (68 lines)
Dear Rod:

I recall a qualitative method from "Spot Tests in Inorganic Analysis" (Feigl) regarding
chromates.  You may need to refer to the text for the exact analysis.  However, as best
I can recall, the method was as follows.  (Incidentally, we used this method as a means
of evaluating the effectiveness of acid cleaners at removing chromate/zincate
conversion coatings during the early development of such cleaners.)

Reagents
Phosphoric/sulfuric acid (75% v/v phosphoric acid (85% w/w) and 25% sulfuric acid (98%
w/w)
di-para-nitrodiphenylcarbazide (0.1% w/w in ethanol)

Procedure
1.  Place 3-4 drops of the phosphoric/sulfuric acid solution on the surface of the
copper to be tested.
2.  Wait 1-2 minutes then add 1 drop of the diphenylcarbazide indicator.  Formation of
a violet color indicates the presence of chromate.

The test should be performed on copper free of chromates to assure no interference from
copper ions.

Regards,

Ted Stern


Rod Semen wrote:

> Does anybody know of a quick test to see if I am removing chromate
> coating on laminate foil? I know about EDX, but I want to do this in
> our lab.
>
> Thanks,
>
> Rod
>
> ______________________________________________________
> Get Your Private, Free Email at http://www.hotmail.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2