Technet,

I'm forwarding this from a colleague.

Cindy Kemp
Lockheed Martin
Orlando, FL
*******************************************************************************

From: [log in to unmask]
Date: Tue, 22 Oct 96 16:35:22 EDT
Message-Id: <[log in to unmask]>
To: [log in to unmask]
Subject: pwb-cca : conformal coating
Sender: [log in to unmask]
Precedence: bulk

hi group;

We are finding that in designs using conformal coating (UR) over plastic parts
that the cc is dewetting on the parts.

Question - is this seen as a problem ?

I am proposing that a note should be added to our designs as follows:

	CONFORMAL COAT DEWETTING ON PLASTIC ENCAPSULATED MICROCIRCUIT
	COMPONENT BODY IS ACCEPTABLE.

If there is a better way please let me here from you.

What is the real would doing ?


			thanx; Skip Greb
========================================================================
To learn more about this email exploder (majordomo), including how to
unsubscribe from this list, send e-mail to: [log in to unmask]
and place the command "help" in the body of the message - subject may be
left blank. Help can also be obtained on the WWW at
http://www.epic.lmco.com/Majordomo
========================================================================

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2