Oups, Ian ; by the sound of it you're in a jam ;
don't get crossed if I see in my crystal ball (one) something what does
not agree with your hard facts :
1)
Somewhere; I think in one of Werner's papers I've read anything less
than 6mm of ceramic on FR4 stands the dilatation's .
That should not be it ; I presume the "problem" is plain crack ; even
without reliability cycling .
2)
Circular cutter ( CAB in V ?) ; or more so still the handling is more
likely ( as you've guessed as well = 0.6 mm end of pad from blade is
highly inconsiderate to the senior cap in question ; I have to say ; you
design fellow likely does not know the blade diagonal stresses in travel
; levered by the size of that thing is sure recipe for crack .
You have my sympathy > hey ; keeps us in job !
3)
The remedy would likely be :
a]
Abandon the circular blade ; it will stress the "design" even if your
operator will feed the panel through on feathers .
Or change the design = move the cap in ; the corner is A brutal place .
b]
If (likely) you can not do anything about design ; than shear ( yes, a
very good guillotine ) will help .
AND feather support ; obviously ;
terrified gentle gender is much more suitable than "confident" handy man
.
May I suggest subsequent use of the French Instrument consequently
utilizing design lad's voluntary cooperation .
c]
break the biscuits PRIOR assembly .
See you Ian
Paul Klasek
colleague on the other side
http://www.resmed.com
> ----------
> From: Ian Squires[SMTP:[log in to unmask]]
> Sent: Wednesday, 4 November 1998 5:34
> To: [log in to unmask]
> Subject: [TN] 2220 ceramic cap failure
>
> All
> Well here it is! my monthly poser for the forum.
> This is one that has come back to haunt me a little, in my first few
> weeks with my current employer i was asked to look at a Small gating
> circuit with a production 'eye'.
> I was unhappy about several of the design features and said so.....but
> being 'johnny come lately' was largely ignored.
> So....we have a board 28mm x 9mm x 0.9mm, populated both sides with
> 0805's, 0603's, SOT23's and a ceramic cap 2220.
> guess what the problem is??? yep the LARGE cap
>
> Cte mismatch between the ceramic and the FR4 in my opinion is too
> much.....agree/disagree?
> The component has one pad running parallel with the long side of the
> PCB 2mm inboard. The other pad runs parallel with the other long side
> of the PCB....0.6mm inboard.
> The boards (50 to a panel) are populated, reflowed both sides and then
> cut out using a circular cutter.
> Pad distance from edge and likely vibration damage are surely
> wrong...agree/disagree???
> Any other possible problems or areas of note would also be appreciated
> as design are still refusing to accept any of this (assuming i am on
> the right track), hard evidence or IPC related docs would be
> appreciated.
> Meanwhile we have a line stoppage and our subcontractor is being
> blamed for poor manufacture. Anyone want to fight their corner with
> me???
>
>
> Regards
> Ian Squires
> Senior Production Engineer
> -------------------------------------------------------
>
> Graseby Dynamics Ltd
> A Smiths Industries Company
> Park Avenue, Bushey, Watford, Herts, WD2 2BW
> Web Site: www.gradyn.co.uk
> Phone: 01923-228566 xt 295
> Fax: 01923-221361
> E-mail: [log in to unmask]
>
> Registered in England no. 480992
> Registered office:
> 765 Finchley Road, London, NW11 8DS
> -------------------------------------------------------
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|