Ramon,
CORFIN Industries is in the business of doing what you ask. They have done
samples for me that look great. NRE per part type is ~ $1000 at ~$5 per
piece depending on lot size of course.
They can be reached at (603) 893-9900, Salem, NH.
Good luck
-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Friday, March 24, 2006 7:18 AM
To: [log in to unmask]
Subject: [TN] Tin Whisker Mitigation
Hello TechNetters:
Does anyone know of companies that are replating parts with Sn63
and reballing BGAs? Could any one share their experiences in
doing this effort? Things such as: extra time needed, cost,
reliability.......
Regards and TIA,
Ramon Dehoyos,
410.552.2210
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|