Hi again Ed,
I started to say "It's me again Margret", but some may not catch the
source of the saying or the implication.
For copper purity analysis help you might try contacting Chrita Dehiptiya,
E-mail address is: [log in to unmask] They do this routinely and she would be glad
to help.
Regards,
Les
> From: "Eltek Ltd. - Process Engineering" <[log in to unmask]>, on
> 1/6/99 5:43 PM:
> Hi technetters
> First of all , thanks for replays concerninging plating of laser drilled
> vias .
> Regardless of it , one of our customers placed request for periodical
> analysis of electroplated copper . I am trying to recall from my memory the
> method , I do remember , that we made it once , but I do not remeber , what
> .
> Regards
> Edward Szpruch
> Eltek Ltd - Israel
> e-mail : [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|