Only  one way I know to eliminate gold slivers and that is to etch first, electroless gold after.

Ed Cosper

----------
From:  Art Shuler[SMTP:[log in to unmask]]
Sent:  Tuesday, October 07, 1997 12:00 PM
To:  [log in to unmask]
Subject:  [TECHNET] Gold Slivers

Does anyone know of a way to completely eliminate gold slivers on a PWB
which is manufactured using a selective gold process? We realize due to
the etch factor, that there will be a 1.4 mil outgrowth when etching 1
oz. copper cladded material.

Mil-P-55110 recognizes that outgrowth will be present on conductors
plated with metals other than solder, but our customer cannot tolerate
slivering.  We've tried brushing them off with a brass wire brush, but
this seems to aggravate the problem.

Any input would be greatly appreciated.

Thank you

Art

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2