Hi, Jim,

I haven't heard of a specific directive banning the use of no-clean, but
having worked all my life in the aerospace manufacturing industry, I
wouldn't naturally us no-cleans to start with.

As has been said before in this forum - no-clean does not mean no-residue.
In the operating environments that expensive aircraft frequent, ANY
residues affect the life and reliability of a board and not predictably so.
Their effect in an aerospace environment is many times more significant
than they are in, say, a PC or VCR, which operate only in relatively very
benign conditions.

If your company is not a specialist CM for aerospace boards - i.e. you're
more commercially oriented - then the directive is possibly issued
specially so that you're not tempted to use no-clean processes.

Peter




                    Jim Jenkins
                    <jjenki09@HAR        To:     [log in to unmask]
                    RIS.COM>             cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     [TN] No No-clean?
                    <[log in to unmask]
                    ORG>


                    02/26/02
                    11:53 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    Jim Jenkins






Hi everybody,

I was just approached by one of our engineers whose customer told her that
the Air Force has issued a directive disallowing the use of no-clean fluxes
on any of their hardware.  The customer is flowing down that requirement to
us.  Do any of you know of this directive or what they could be referring
to?

Thanks,

Jim

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2