I am experiencing solderability problems due to my oven glue procurement at
the wave solder.  My pads are nice and shiny before the oven then they come
out with a haze that can't be wiped off or cleaned off with alcohol.  Is
there anything that I am missing that could be caused by the oven?  Would
nitrogen help this?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2