I've also seen SnPb slivers come out of holes if a screw is ever removed after its initial insertion. It’s a short waiting to happen.
Dick Krug, CSMTPE
SMT Process Engineer
Sparton Corporation
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro
Sent: Monday, May 02, 2011 1:19 PM
To: [log in to unmask]
Subject: [TN] Mounting holes with plated barrels
I was reviewing a new design and found the mounting holes have plated barrels.
In my past, I have always steered Design away from plating the barrels of PWB holes used for mounting holes (and torque).
Far back in my memory, I remember experiments I had run which revealed that the HASL solder on the mounting hole annular ring allowed solder creep making the fasteners come loose over time. I also seem to remember something about not wanting to put a barrel in compression. This is a double sided board mounted to a copper plate and the entire assembly is tin lead plated and then fused. On a multilayer board, the argument is easily made to not compress the internal layers.
I am looking for something in the standards which might provide some direction against this type of design.
The only stated reason from the mechanical designer was increased thermal dissipation, for which my argument is that the fastener provides much more capacity for transfer than does the barrel wall.
Am I being too conservative?
Phil
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|