For starters -- congrats to you and Chris and best wishes for a long and
happy union!
I've been experiencing some soldering challenges these days with a myriad of
component lead surface finishes.
One inquiry to an inductor mfr "what is the base metal and surface finish"
yeilded a response "platinum/palladium/silver". Typically, I've been
seeing, outside of TI's Palladium, Sn80Pb20 and Sn85Pb15 platings but none
(to my knowledge) have been 100% silver.
My initial recourse was to revamp each reflow profile for a higher reflow
temp (230°C) and longer dwell time (upwards to 60 sec) coupled with standard
Sn62 solder paste (although I would prefer to have the Sn62 with Sb).
As was mentioned during the infamous "IMC string", the CuAg intermetallics
are definitely something to not be overlooked -- as you know more on this
subject than I.
If I come across any peculiar finishes, I'll keep you posted.
Regards,
Steve Sauer
-----Original Message-----
What I am really concerned about right now is component manufacturers, who
in their rush to be lead free, have resorted to using thick, 100% silver
lead finishes. Have any of the rest of you run into this recently?!
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|