TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jeff Hempton <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 27 Oct 1998 13:45:10 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Chuck,
  We perform heat seal here with much success. It can be performed on either
gold plated fingers (expensive) or carbon coat (if your vendor has the
capability). From our resident guru, who comments:
     You should expect a 99/44/100% heat seal success rate. Call me at
     219-358-3386 and we can talk.

                                        Larry Marks

     Good luck, Jeff Hempton/Larry Marks
     United Technology Electronic Controls

______________________________ Reply Separator _________________________________
Subject: [TN] Heat seal connectors to LCD
Author:  Jeff Hempton at Carrier-HUN-CED1
Date:    10/26/98 12:52 PM


     Hey guys, do you wish to respond to this TechNet question???


______________________________ Forward Header __________________________________
Subject: [TN] Heat seal connectors to LCD
Author:  Chuck Garth <[log in to unmask]> at Internet
Date:    10/26/98 10:20 AM


I am having a major problem attaching heat seal ribbon to lcd's and gold
plated circuit board fingers.  Can anyone tell me what can of success rate I
should expect?
What can I do to assure connection reliability?  Such as chemical cleaning or
any thing else.
Any information on this subject would be appreciated, contacts, etc.
Chuck Garth

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2