TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 31 Mar 2010 08:12:59 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Blair Hogg <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="windows-1252"
Content-Transfer-Encoding:
quoted-printable
From:
Blair Hogg <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
I have the understanding that pink poly, while being a non-generating 
material, does not or is not as good at protecting devices from static 
discharges as conductive black or metalized film. Am I mistaken or is this not a 
concern in this application?

Blair

On Tue, 30 Mar 2010 07:04:05 -0700, Gregg Owens 
<[log in to unmask]> wrote:

>Dear TechNet:
>
>There has been discussion on the use of "pink poly" for ESD prevention on 
flight hardware. An expressed concern has been the chemicals added to the 
surface of pink poly can potentially contaminate our products with the residue 
pink poly leaves behind. I have posted a picture of one of our boxes which 
have both the pink poly and black ESD style of cap plugs. What are any of 
your experiences with contamination associated with using pink poly? As 
always, thanks,
>
>Gregg Owens
>Technical Writer - Avionics
>Space Exploration Technologies Corporation
>1 Rocket Road | Hawthorne | CA | 90250
>310-363-6533 | [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2