TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 18 Mar 1999 08:38:44 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
In a message dated 3/18/99 5:20:58 AM Pacific Standard Time, edward-
[log in to unmask] writes:

>   Hi,
>       Has anyone done any studies for the change of depth of solder paste
>       with wear on the stencil. Metal blade squeegees damage the stencil
>       over a period of time, yielding an uneven surface in the form of
>       furrows in the direction of travel. Any uneveness in the stencil is
>       going to hold the blades that much further off the board giving more
>       solder paste.
>       Any comments?
>       Regards
>       Edward Brunker

Hi Edward,

     I was told once by a gentleman named Bob Jillings, the owner of a stencil
company called Screen Manufacturing Technologies (since bought by Alpha
Metals), that he would guarantee his stencils for at least 10,000 prints. Not
quite sure if the guarantee was based on the bond of the mesh to the foil and
frame, or the foil itself...but that's all I've ever heard. I'll admit after
thinking about it though, I've used stencils for more than 10,000
prints...stencil did look pretty used after that many prints. I don't know if
this helps or not...

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2