Cal,
You should seriously consider sending several to some labs to determine
what sort of contaminants are present.
1. No Clean is a misnomer It should read No Flux Removal. Depending on
the Class (1, 2, or 3)
the cleanliness requirements of the components and boards must be
determined prior to soldering .
2. You have no idea where these parts have been stored, or how they've
been handeled, or how many
times they've been repacked and shipped.
Are they $9,000 apiece or is the whole lot valued at that?
David A. Douthit
Manager
LoCan LLC
Cal Driscoll wrote:
>Hello All-
>
>We have 200 QFP components that failed a Kester wet balance test method
>using Kester RMA Flux.
>Unfortunately, I do not know the nature or origin of the residue/
>contamination.
>
>Data:
>- We use a no clean process (if they did not wet with RMA can not imagine
>them wetting with NC).
>- 240 Pins with 20 or 26 mil pitch
>- Parts are MD'd (Manufactured Discontinued)
>- Value $9,000
>
>I am looking for direction and recommendations.
>
>Input on recommended labs is also Valuable.
>
>Thanks in advance,
>Cal
>
>Caldon Driscoll
>Program Manager, Circuit Board Manufacturing
>CTDI
>1373 Enterprise Drive
>West Chester, PA 19380
>610-793-8098
>WWW.CTDI.COM
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|