TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 16 Apr 2008 14:48:43 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Subject:
From:
Mike Sewell <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<6AF520ECAE2FD611BF8E00C09F065566CCFB7F@server>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (56 lines)
How slow can you run your reflow oven?  Can't put too many in
though...might let you see if this fixes your problem.

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Wednesday, April 16, 2008 1:33 PM
To: [log in to unmask]
Subject: Re: [TN] Out Gassing

Hi Bob,

Thanks for the great information and videos. I've heard about out
gassing
for more years than I'd like to admit but that's the first time I've
seen
it, Great Stuff!!!

Jon suggested 125C for two hours as a corrective bake. In your article
you
mentioned bake but no specifics. Like I said in an earlier email, we can
only go to 140F, will that do anything?

Thanks again,

KennyB


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2