I apologise in advance for taking this thread off on a slight tangent
but how do you check sub micron plating thickness to any degree of
accuracy? I have often been told that it is very difficult to do.
Kane, Amol (349) wrote:
> In case of ENIG, the Ni and the Au thickness would be important too wont it?.....the idea here is (or what I thought would be) is to monitor the plating process of the supplier and compare it to the max and min specs of Ni and Au given in 4552 to ensure that you consistently get boards that will not be susceptible to Au embrittlement on one end to black pad on the other........seemed logical to me, and therefore wanted to know if this was a practice in the industry........
>
> Amol
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
> Sent: Tuesday, March 13, 2007 10:27 AM
> To: [log in to unmask]
> Subject: Re: [TN] PCB plating Qualification
>
> Hi Amol,
> I would be very much surprised if there were such efforts. Why undertake such
> an effort?
> The only plating thickness that is really critical is the copper plating
> thickness in the vias-and it will vary according to all kinds of variables.
>
> Werner
>
>
>
> **************************************
> AOL now offers free email to everyone.
> Find out more about what's free from AOL at http://www.aol.com.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> CONFIDENTIALITY NOTICE:
> This e-mail, and any attachments, is for the sole use of the intended
> recipient(s) and may contain information that is confidential and
> protected from disclosure under the law. Any unauthorized review, use,
> disclosure, or distribution is prohibited. If you are not the intended
> recipient, please contact the sender by reply e-mail, and delete/destroy
> all copies of the original message and attachments.
> Thank you.
--
Eric Christison Msc
Mechanical Engineer
Home Personal, Communication Sector
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|