TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Tue, 13 Jan 2009 18:55:48 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (101 lines)
Sklenar,
You can't use an XRF to tell the dufference between IPA and water. 

My first suggestion is smell. 

Second - FTIR. 

Bev
RIM

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Jan 13 18:36:52 2009
Subject: Re: [TN] Water and Alcohol Flux

Did you try  a digital pH meter  to see if any difference between these two fluxes is recordable?
Another option could possible  be the spectrum  comparison if you have a XRF  analyser  or something similar available...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna
Sent: Wednesday, 14 January 2009 10:35 AM
To: [log in to unmask]
Subject: Re: [TN] Water and Alcohol Flux

A bic lighter...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Larry Dzaugis
Sent: Tuesday, January 13, 2009 6:16 PM
To: [log in to unmask]
Subject: [TN] Water and Alcohol Flux

What is a simple test to tell the difference between alcohol and water
based
fluxes?
Both are 3% solids flux.

I am running both fluxes in the same machine.
The concern is that the wrong flux is loaded during a change over.
They behave so differently that the use of the wrong one will result in
badly soldered boards.

Our long term solution is seperate flux tanks and spray nozzels if it
continues with bar code verified replenishment.

In the mean time what would be a quick test?

The weight of an alchol flux on the PCB is inconsistent due to
evaporation.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2