On 25, June, the question was asked:
>> I am looking for a temporary way to mark defects on a PCB assembly (other
than the >> red arrows that everyone uses). The boards will go back through a
water wash, so I >> was thinking a water soluable, non-conductive ink would
be nice. Are there any >> recommendations?
Good day there!
Yes, Marshall's (www.marshall.com) carries some markers from Tech Spray
that are called solder-fault markers (PN# 1850-O for orange ones, 1850-W for
white ones), and they're listed at $5.05 each, they contain 10ml of the
marking agent that is said to be non-stringing, quick drying, and can be
cleaned either with warm water or solvent. The agent also contains a black
light indicator so if you really want to be sure you don't miss anything you
can use a black light to make things jump out at you...
-Steve Gregory-
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|