TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Peter Swanson <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 3 Jan 2007 15:43:45 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Burtt, Nigel" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Content-Transfer-Encoding:
quoted-printable
From:
"Burtt, Nigel" <[log in to unmask]>
Parts/Attachments:
text/plain (105 lines)
Peter,

          I guess in part that is what I am asking. Do US assemblers

more commonly use the in-house/DIY approach rather than have the PCBs

supplied with the masking pre-applied to a supplied (gerber layer?)

pattern. Alternatively I know that some use masking that is removed by a

post-wave-solder cleaning process rather than peelable. Just surprised

that what our suppliers seem to think is not a big problem to provide as

a normal service is apparently not so readily available in USA... Or

maybe it just depends who you ask!



Cheers





Nigel Burtt 

Production Engineering Manager 

Dolby Laboratories, Inc. - European HQ 

Email: mailto:[log in to unmask] 

Tel:     +44 (0)1793 842132 [direct line with voicemail] 

Fax:    +44 (0)1793 842101



 



-----Original Message-----

From: Peter Swanson [mailto:[log in to unmask]] 

Sent: 03 January 2007 15:37

To: TechNet E-Mail Forum; Burtt, Nigel

Subject: RE: [TN] Temporary peelable solder masks



Nigel,



You rightly draw the distinction between a) the types of temporary masks

which are pre-applied by screen printing, usually by the pcb fabricator

and b) the temporary masks which are dispensed on by the guys doing the

assembly. They are different.



Whilst it is obviously desirable to have this job done by your fab guy,

as you pointed out, it isn't always straightforward. In particular, I

remember a few years back when the process window on the screenable

materials wasn't very wide, resulting in problems from under/over cure,

removal, etc. Maybe the formulations are more robust today.



It is possible to make the "in-house" dispensable types more appealing.

Dispensing can be by fairly inexpensive robotics. Curing can be quick by

heat or UV. Is this approach an option?



Regards,

Peter

--------------------------------------------------------

Peter Swanson           [log in to unmask]

INTERTRONICS                http://www.intertronics.co.uk

Tel: +44 1865 842842                   Oxfordshire, England



INTERTRONICS is dedicated to providing quality material, consumable and

equipment solutions to the high technology, high performance assembly

industries, incorporating outstanding levels of technical support and

customer service.



Read our blog! http://www.intertronics.co.uk/blog/blog.htm



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of N Burtt

Sent: 03 January 2007 09:27

To: [log in to unmask]

Subject: [TN] Temporary peelable solder masks



I'm being told that these are not widely used in USA, the common types

used here in the UK (Peters and Electramask) not readily available, and

they create packaging and shipping problems... thus US PCB suppliers

reluctant to supply PCBs with peelable masking applied. Is this true?



Now they are by no means a perfect solution to protecting holes on a PCB

during wavesolder, but am not aware of another way of doing so in a

no-clean RoHS process if fixturing can't do it. What do US PCB

assemblers do if pre- applied peelable masking is really not viable?

Other ideas?



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

-----------------------------------------

This message (including any attachments) may contain confidential
information intended for a specific individual and purpose.  If you
are not the intended recipient, delete this message.  If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2