TECHNET Archives

July 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 18 Jul 2018 22:13:51 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dennis Fritz <[log in to unmask]>
Subject:
From:
Dennis Fritz <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
NTC - Yep, you EEs keep on thinking you are in charge.   Meanwhile, my
minions and I will keep on sneaking up on you - "The future of electronics
is chemical"
https://phys.org/news/2018-07-future-electronics-chemical.html

On Wed, Jul 18, 2018 at 7:22 PM Yuan-chia Joyce Koo <[log in to unmask]>
wrote:

> that's scary.
> On Jul 18, 2018, at 11:48 AM, John Maxwell wrote:
>
> > High dielectric constant ceramic capacitors all exhibit aging due
> > to the crystal structure changing from ferroelectric (tetragonal or
> > diamond) to paraelectric (cubic) structures. Higher the dielectric
> > constant (k) and the thinner the dielectric the more rapidly the
> > parts age or lose capacitance.
> >
> > John
> >
> >
> > Sent from my iPhone
> >
> >> On Jul 18, 2018, at 11:10 AM, Guy Ramsey <[log in to unmask]>
> >> wrote:
> >>
> >> Well, I'll Be.  I cooked them at 150C for an hour and they measure
> >> 100uF
> >> I learned something today.
> >>
> >>> On Wed, Jul 18, 2018 at 8:08 AM <[log in to unmask]> wrote:
> >>>
> >>> Guy,
> >>>
> >>> Read this and try putting the parts through their Curie point and
> >>> test
> >>> them again.  We have seen this on some parts here.
> >>>
> >>> https://www.johansondielectrics.com/ceramic-capacitor-aging-made-
> >>> simple
> >>>
> >>> Drew
> >>>
> >>> -----Original Message-----
> >>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
> >>> Sent: Wednesday, July 18, 2018 7:00 AM
> >>> To: [log in to unmask]
> >>> Subject: [TN] capacitor measurement
> >>>
> >>> I got pulled into a Receiving Inspection problem. Our test
> >>> instrument, an
> >>> old HP 4192A impedance meter, and a newer Instek 6020 tell us
> >>> that our X5R
> >>> capacitors are out of spec.
> >>> A 100uF, 10%, 6.3V capacitor measures between 25% and 30% below the
> >>> nominal value.  The instruments have Kelvin probes and are zero
> >>> calibrated
> >>> at frequrency, 120Hz the test waveform is 500mV rms.
> >>> Does anyone have any advise?
> >>>
>