TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Dave Hillman <[log in to unmask]>
Date:
Tue, 10 Sep 2002 07:26:15 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (88 lines)
Hi Carrie! Just a word of caution on what chemistry you select for cleaning
the aluminum - anodized and chromated (e.g. chemical conversion coatings)
finishes can be damaged depending on the temperature/chemistry combination
you use. There are plenty of industry papers documenting the detrimental
impact of temperatures above 150F in combination with high pH cleaning
chemistries. I recommend you specification ask the potential chemistry
suppliers what the impact on the anodized and/or chromated coating could
be. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





"Morse, Carrie" <[log in to unmask]>@ipc.org> on 09/09/2002 03:24:57 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to "Morse, Carrie" <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Cleaning Aluminum


I am looking for a cleaning solution to be used in conjunction with our
Ultrasonic cleaner that will
remove organics (such as finger oils) from machined aluminum parts.  Some
of the parts are
straight aluminum (untreated), some are clear anodized, and some are clear
chromated.
Preferably, I'd like to find one cleaner to fit all.

We are currently using Branson's MC-3 which is far too harsh and has
resulted in aluminum
oxide deposits and/or tarnishing even after repeated attempts to decrease
time and dilution
per the mfr's recommendation.

At this point I'm ready to use some Joy Dishwashing detergent, but, would
rather use a product
designed for industrial use that cost 100 times more so the customer's
perception  of our
cleaning process will be enhanced :)

Due to the nature of the product these parts go onto, "cleanliness" cannot
be determined until
after an entire unit is built and tested.  Therefore, I'm simply looking
for companies that sell cleaners that
are intended to remove organics and I'll have to build samples and have
them tested at the customer site.
(oh what fun!)

Thanks,
Carrie

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2