TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wWH6g-000BjAC; Tue, 27 May 97 02:55 CDT
Content-Type:
text/plain; charset=ISO-8859-1
Old-Return-Path:
Date:
Tue, 27 May 1997 16:12:39 +1000
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12934
X-Status:
TO:
"Therese M. Kokocinski" <[log in to unmask]>
X-Loop:
Return-Path:
<TechNet-request>
X-Priority:
3
Content-Transfer-Encoding:
7bit
>From bergdi Tue May 27 02:
56:03 1997
X-Mailer:
Microsoft Internet Mail 4.70.1155
Resent-Message-ID:
<"kEzl3.0.kO9.1EfYp"@ipc>
Subject:
From:
"David Taylor" <[log in to unmask]>
X-MSMail-Priority:
Normal
Cc:
"Technet" <[log in to unmask]>
From [log in to unmask] Tue May 27 09:
06:55 1997
Message-Id:
Parts/Attachments:
text/plain (25 lines)
Therese,

Have a go at printing peelable soler mask over your gold contact fingers.

We have had success with this using a piece of routed entry board in lieu
of using a screen to print through.

Regards,
David Taylor
Chief Engineer
East Coast Printed Circuits
61 2 9982 1377 Phone
61 2 9971 0437 Fax

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2