A few years ago I plated a bunch of boards wirh all tin for an OEM who
built product with them.  A "short" time thereafter, the product all bombed
out from shorts created by tendrites of tin.  The OEM was embarassed,
out a lot of money and learned their lesson.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2