Dear Technetters,
For our stencils I have recently introduced the homeplate design for the apertures of chipcomponents larger than 1206.
But now a problem occurs with the guys who have to order the stencils: it takes a lot of time, by using Gerber data, partslist and assembly drawing to figure out which components are 1206, 1210, 1812. For a coil or tantalumcaps with such a footprint I don't want a homeplate aperture because these parts need a little more solder.
So we end up with a nice specification, but very unpractical for the production engineers.
How do others deal with this ? Mabe you have suggestions on how to make an easier-to-use specification ? Or ideas about easier ways to order a stencil according to my spec ?
Should I keep it simple and say "use homeplate-apertures for all footprints larger than 1.5 * 1.5 mm ?"
Daan Terstegge
SMT Centre
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|