This is incredible. Insects and their acetic acid deposits.

You know I love you babe but Graham - do I have to worry about my embedded
pacemaker in the same way? Of course I do because of my cave's environment.
I got to get me some CAF or was that COW. No matter, I do have a cramp in my
CAF.

I'm goig to be good from now on. I promise but don't hold me too it.

I do have a serious question though, as you serve on the CAF committee. How
good really is a conformal coating to keep moisture out to prefent the CAF
effect? Also, if we dry the boards sufficiently, how good will conformal
coating be especially if the boards are, how shall I say, vacuum sealed with
dessicators and moisture indicators?

I really have to find some work or fish,

MoonMan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2