We apply our white ID silk screen  Before Hasl.

Jim Herard
KBL, Product Quality Engineering
IBM Microelectronics Endicott
t/l 857-7026

---------------------- Forwarded by Jim Herard/Endicott/IBM on 06-27-97 12:01 PM
 ---------------------------

        [log in to unmask]
        06-27-97 11:56 AM
Please respond to [log in to unmask] @ internet

To: [log in to unmask] @ internet
cc:
Subject: Idents before or after HASL

What is the most common practice:

Silkscreen idents before or after HASL?

I would appreciate any comments on this.

thanks -

Jamie McIntyre
PCI
Toronto, Canada

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2