TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jim Trainor <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 8 Jan 1999 09:15:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
-----Original Message-----
From:   Neil Atkinson [SMTP:[log in to unmask]]
Sent:   Friday, January 08, 1999 2:51 AM
To:     [log in to unmask]
Subject:        Re: [TN] immersion white tin finish
Importance:     High

        The comments on Omikron fit with what we have found.  This seems
to be the better of the immersion tin finishes and certainly seems to be
as good as a good HASL finish.  (not all HASL finishes are actually that
good!)

        We are a UK company and our trials with certain other immersion
tins have proved disappointing even though they seem to have sold quite
well in the states.

        The biggest problem we seem to have is people (customers) appear
to have been brain washed into believing HASL is THE finish to have and
it is extremely difficult convincing people that it is not the be all
and end all.

[Jim Trainor]

Initial testing of the Omikron finish using a meniscograph show good
wetting forces but once exposed to humidity conditioning of 85C/85RH,
solderability deteriorates due to oxidized  copper tin intermetallics on
the surface.If there were a guarantee of using this finish within a week
then it could be a good finish.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2