TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Grossmann, Guenter" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Grossmann, Guenter
Date:
Fri, 6 Jul 2012 15:07:00 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
Graham

I agree. I even would say that conformal coating might well promote the growth of dendrites if the PCBs are not cleaned well ahead of the coating.

Günter Grossmann



>-----Ursprüngliche Nachricht-----
>Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Graham Naisbitt
>Gesendet: Freitag, 6. Juli 2012 14:23
>An: [log in to unmask]
>Betreff: Re: [TN] Copper Dendrites
>
>Hi Neil
>
>I stand by my earlier posting on this. Neither a solder resist nor a
>conformal coating will PREVENT dendrites, they might delay it for a
>while, but then what is lurking and festering underneath..just when you
>thought it was safe to go back in the water!?
>
>Graham Naisbitt
>
>
>On 5 Jul 2012, at 19:50, Neil Atkinson wrote:
>
>> Thanks everyone for comments so far - haven't been on Technet for a
>while so it was good to get such good responses.
>>
>> Really miss Werner for questions like this...
>>
>> Actually we have never seen a failure for dendrites; however, we have
>a customer who has a past problem with another supplier due to dendrites
>on PCBs and as a result wants us to cover vias with solder resist or
>conformal coating.
>>
>> Tha,
>>
>> Neil
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud
>service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud
>service.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2