John - We had problems with very low leakage current photomultiplier tubes
(on the order of a few femto-amps). No matter how we cleaned/treated the
PCB there was always enough cinductivity (on the surfaces, I guess) to
swamp out the PMT signal. Our solution was to put the critical components
on teflon standoffs swaged into the PCB. The final assembly was washed with
de-ionized water as a final rinse. On earlier circuits with less sensitive
PMT's cleaning and conformal coating was sufficient. I don't know if this
helps you with your customer but We've hit are times when extreme cleaning
is necessary.

Ray Klein

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2