Michael
Are you talking process defects only, or including test failures that could
not be caught downstream? I'll assume you are considering process defects
only.
I believe that you have to consider the device types on the board in any
target - as a crude example, a board covered with 1206 resistors is easier
than 0603's, and a BGA will give you a better process yield (typically) than
a big QFP module. And the other twist is the inspection criteria - an
amazing yield at class 1 is not so hot at class 3.
If it were me I would base my cut-off on a decreasing target that is
realistically based on past history, expectations, board complexity, design
issues, and rational thought. At another employer I was on the other side
of this fence, with a customer who had a target and didn't care how well
thought out it was, it was THE target and that was it.
good luck!
- Graham Collins
-----Original Message-----
From: Michael Forrester [mailto:[log in to unmask]]
Sent: Tuesday, September 08, 1998 5:15 PM
To: [log in to unmask]
Subject: [TN] Acceptable PPM Defect Rate
I am a floor shop engineer for a Digital Oscilloscope line. Our PCA's have
mixed technology and down to 20 mil. (typically 25 mil and above).
Typically the boards are 12" X 12" with approx. 10K chances for error (ie.
Comp. Count + Lead Count). Typically 10% of the parts are located on the
secondary side. I would like to know what the industry considers an
acceptable defect rate in PPM coming into a subassembly test department,
after an in-house QA lot inspection, and rate from an outside PCA house.
My QA department has a certain threshold in mind before something is a
"problem". I want to know if their threshold is at least in the ballpark
of the industry. Thank you.
Best Regards,
Mike Forrester
LeCroy Corp.
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|