Agree with Phil , it's basically a flash plate , and not quite to last
century standards,
but as i stated previously few times :
Horses for courses (commerce/applications)will dictate specifications more
and more :
i opted out of selective platings decades ago , and that time it was a MIL
heresy :
validated (NiAu) with 1M+ cycles in both telecom and med. boards .
Sounds like you have commercial application at hand with some 5-10y life
span;
with fairly set connectivity: with little justification of building to
higher application standards.
You may be correct that it is indeed conversion goof ,
but looking back i never gave an ounce unless i proved (enviro/cycled) it's
needed.
VP used to shake his head as well ("you can't go this low"),
but some say the proof is in the pudding ;
saved millions by now by designing to the task (aka toyota) .
Overchromed monuments ain't gonna to fly in 3M with design cycles 6-12
months .
Just a practicioner's opinion Ken
(got a compliment once as "real" engineering)
Composites in general went that way decade ago .
Check intentions
paul
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Friday, 3 March 2000 9:08
To: Paul Klasek
Subject: Re: [TN] Help on Fab note related to gold finger
Gold plating thickness. I thought it is too low as we even specify 3-8
micron inch on Ni-Gold board. .00003" is 30 micro-inch which I considered 3
micro-inch. Conversion goof-up.
Thanks for the help.
re,
ken patel
At 08:56 AM 3/3/2000 +1100, you wrote:
>Sounds fine for a connector sliding onto gold fingers even on regular
>(daily) base
>(the connector will outlast the fingers)
>What made you doubt it ken?
>
>paul
>
>-----Original Message-----
>From: Ken Patel [mailto:[log in to unmask]]
>Sent: Friday, 3 March 2000 8:38
>To: [log in to unmask]
>Subject: [TN] Help on Fab note related to gold finger
>Importance: High
>
>
>I received a new drawing which states the following note:
>
>Edge connector: Phosphor Bronze with .00003" minimum gold over .00005"
>minimum Nickel, both side.
>
>Is it sound OK as this is applicable to gold finger?
>
>re,
>ken patel
>______________________________________________________
>Ken Patel Phone: (408) 490-6804
>1708 McCarthy Blvd. Fax: (408) 490-6859
>Milpitas, CA 95035 Beeper: (888) 769-1808
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
>
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|