Another cause could be soldermask on the pads. A thin film of soldermask
gives the appearance of exposed copper.
Rick Howieson
GTC
>-----Original Message-----
>From: McMonagle, Michael R. [SMTP:[log in to unmask]]
>Sent: Tuesday, November 02, 1999 12:28 PM
>To: [log in to unmask]
>Subject: [TN] Exposed Copper on Fabs
>
> I need a little insight from those of you in the fab end of the
>industry regarding an issue we have seen on a few incoming fabs. They are
>processed by the supplier using a horizontal HASL process, and we are
>finding random instances of partially or fully exposed copper on pads.
>Meaning, you may have one pad out of a row of a QFP pattern or one pad out
>of an entire BGA array that is bare copper even though all
>adjacent/surrounding pads are fully covered with HASL. Is this something
>inherent in the horizontal HASL process? If so, what is the phenomena that
>causes it? If not horizontal HASL processing, what are other potential
>causes? I have my ideas, but am looking for others. Enquiring minds want to
>know....
>
>Mike McMonagle
>PCA Process Engineering Supervisor
>K*Tec Electronics
>1111 Gillingham Lane
>Sugar Land, TX 77478
>(281) 243-5639 Phone
>(281) 243-5539 Fax
>[log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|