In a message dated 2/15/2001 8:46:23 PM Central Standard Time,
[log in to unmask] writes:
<< Solder paste reuse: does anybody has this practice? Obviously, my solder
paste supplier does not recommend it.
Nicolas Ortiz
Process Engineering Group Leader
Conexant Systems >>
Hi Nicolas,
Your supplier is not recommending it to in order to sell you more paste, it
is a valid recommendation.
I'm not quite sure about what you mean by "reuse", but if you mean taking
paste off a stencil, putting it back in a jar after a run, and then keep
using it, that's a bad idea.
The paste will absorb moisture, the volatiles in the paste will evaporate,
basically changing everything about the formulation of the paste = not
performing like it's been advertised to do...I don't know of any manufacturer
of solder pastes that would recommend to reuse solder paste after it's been
dispensed on a stencil...
I do however, understand your concern about the expense when throwing away
solder paste...it's not cheap, anywhere from $50.00-75.00 for a 700-gram jar.
But you can recover some of the costs through recycling...Alpha/Fry Metals
will recycle solder paste and give you back the money that the tin/lead
market prices are at the time you turn it in...
Bottom-line, don't "reuse" your solder paste...it'll bite you...
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|