WE ARE USING A LPISM AND HAVE PASSED BOARDS TWICE THRU THE DEVELOPER
ie MADE SURE THERE IS NO MASK LEFT ON THE PADS
PRE CLEANER IS FERRIC HLORIDE WITH HYDOCHLORIC AND PHOSPHORIC ACID
please note the bottom side is ok .It is the top side which has the problem
On Wed, 25 Nov 1998, George Toman wrote:
> Afri,
>
> Two questions in reference to your inquiry:
> 1. What type of solder mask are you using?
> 2. Could you describe your process for cleaning prior to flux application?
>
> Regards,
>
> George Toman
> Circuit Center Inc.
> phone: 937-435-2131
> fax: 937-435-7698
> e-mail: [log in to unmask]
>
> ----------
> > We have a horizontal solder leveler and are having to pass some boards
> > twice thru ,because it does'nt cover some of the fine pitch surface mount
> > pads on the first pass.
> > Has anyone out there had this problem and what is the best fix.
> > thanks
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following
> > text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> > for additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> > 847-509-9700 ext.312
> > ################################################################
> >
> >
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|