TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Tan Geok Ang <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 4 Nov 2008 19:10:09 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Charming Chan <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="GB2312"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Hello Ang, 



Info as follows, sorry for late. Thanks.



a) What alloy is being used?

SAC305



b) What type of flux is being used?

Alpha EF-8000



c) What is the plating finish?

OSP, ENIG



d) What is the board thickness?

1.6mm generally



e) What is the pin-to-hole rate?

0.7874mm hole size, 0.55 lead size



f) Can you send me (off-line) the PTH design and connector Mfg P/N used?

0.7874mm hole size, 1.397mm pad size, 0.55mm lead size



Best Regards

Charming Chan

PCBA Engineer













"Tan Geok Ang" <[log in to unmask]>





2008-10-29 09:16

 

        收件人:        "TechNet E-Mail Forum" <[log in to unmask]>, 

<[log in to unmask]>

        抄送: 

        主题:  RE: [TN] How to improve solder filling and wetting contact 

angles for thermal vias at wave soldering process.





Can you provide with the following

a) What alloy is being used?

b) What type of flux is being used?

c) What is the plating finish?

d) What is the board thickness?

e) What is the pin-to-hole rate?

f) Can you send me (off-line) the PTH design and connector Mfg P/N used?



Thanks!



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Charming Chan

Sent: Wednesday, 29 October 2008 8:59 AM

To: [log in to unmask]

Subject: Re: [TN] How to improve solder filling and wetting contact angles 

for thermal vias at wave soldering process.



Hello Ang, 



Thanks a lot for your input. Please refer to the comments under your 

proposals. We really did the work the same as you proposed but still poor 

solder filling in the through hole barrel with thermal pad, and the 

wetting contact angle exceed 90°.



Do any other assembly shops have the same issue? How to improve? Thanks.



a) Redesign the thermal pad  grounding so that it is not fully contacted 

with the thermal layer.

[Comments] In our design, to facilitate wave soldering, where a component 

through hole is supposed to connect to copper plane, a thermal relief pad 

is designed always.



b) At solder during the SMT process (ensure that the pin is still able to 

insert into the hole).

[Comments] Yes, it is.



c) Increase the preheat to even out the whole board 

[Comment] Tested with dip tester, the preheat temp. is about 120C, and the 



conveyor is set at 80cm/min.



d) If the space/distance between chip wave and main is too far, do not 

turn on the chip wave.

[Comment] Chip wave turn off.



Best Regards

Charming Chan

PCBA Engineer











Tan Geok Ang <[log in to unmask]>

发件人: TechNet <[log in to unmask]>





2008-10-28 22:00

请答复 给 TechNet E-Mail Forum; 请答复 给 Tan Geok Ang

 

        收件人:        [log in to unmask]

        抄送: 

        主题:  Re: [TN] How to improve solder filling and wetting contact 



angles for thermal vias at wave soldering process.





a) Redesign the thermal pad  grounding so that it is not fully contacted 

with the thermal layer.

b) At solder during the SMT process (ensure that the pin is still able to 

insert into the hole).

c) Increase the preheat to even out the whole board 

d) If the space/distance between chip wave and main is too far, do not 

turn on the chip wave.



________________________________



From: TechNet on behalf of Charming Chan

Sent: Tue 10/28/2008 8:25 PM

To: [log in to unmask]

Subject: [TN] How to improve solder filling and wetting contact angles for 



thermal vias at wave soldering process.







Hello TechNet experts,



At the wave soldering process, the solder filling of thermal vias(the via

holes connected with copper plane by thermal pad) can not fulfill the 75%

acceptance spec in IPC-610D. Moreover, at the lead free wave soldering

process, the wetting contact angles of thermal pads exceed 90° often.



My question is how to improve solder filling and wetting contact angles

for thermal via holes? Thanks a lot.



Best Regards

Charming Chan

PCBA Engineer









--------------------------------------------------------

ZTE Information Security Notice: The information contained in this mail is 



solely property of the sender's organization. This mail communication is 

confidential. Recipients named above are obligated to maintain secrecy and 



are not permitted to disclose the contents of this communication to 

others.

This email and any files transmitted with it are confidential and intended 



solely for the use of the individual or entity to whom they are addressed. 



If you have received this email in error please notify the originator of 

the message. Any views expressed in this message are those of the 

individual sender.

This message has been scanned for viruses and Spam by ZTE Anti-Spam 

system.







---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 



for additional information, or contact Keach Sasamori at [log in to unmask] or 



847-615-7100 ext.2815

-----------------------------------------------------









--------------------------------------------------------

ZTE Information Security Notice: The information contained in this mail is 

solely property of the sender's organization. This mail communication is 

confidential. Recipients named above are obligated to maintain secrecy and 

are not permitted to disclose the contents of this communication to 

others.

This email and any files transmitted with it are confidential and intended 

solely for the use of the individual or entity to whom they are addressed. 

If you have received this email in error please notify the originator of 

the message. Any views expressed in this message are those of the 

individual sender.

This message has been scanned for viruses and Spam by ZTE Anti-Spam 

system.









--------------------------------------------------------

ZTE Information Security Notice: The information contained in this mail is solely property of the sender's organization. This mail communication is confidential. Recipients named above are obligated to maintain secrecy and are not permitted to disclose the contents of this communication to others.

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the originator of the message. Any views expressed in this message are those of the individual sender.

This message has been scanned for viruses and Spam by ZTE Anti-Spam system.


ATOM RSS1 RSS2