The only time we experience this problem is when the board supplier quality
is poor. Try doing a solder shock at 288 C for 10 seconds then microsection.
If you see trace separation, reject the boards to your supplier and tell him
to get his act together.
Bryan Kerr
Alenia Marconi Scotland
----- Original Message -----
From: Art Fisher <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 27, 1999 8:08 PM
Subject: [TN] Traces
> Has anyone experienced problems with inner traces separating from barrels?
> How much does excessive heating during hand soldering contribute to this?
> Art
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|