TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Lustig, Steven K.." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 6 Oct 1999 08:31:50 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Matthias,

No, I am refering to adhesive bonding of a large part (a metallic spring
finger in fact).

-Steve


Steven K. Lustig
Process Engineer
EMS Technologies, Inc.
Norcross, GA
(770) 263-9200 x4714
[log in to unmask]


-----Original Message-----
From: Matthias Mansfeld [mailto:[log in to unmask]]
Sent: Wednesday, October 06, 1999 10:29 AM
To: Lustig, Steven K..; [log in to unmask]
Subject: Wire(?) Bonding, was: Re: [TN] Temporary Solder Mask


On  6 Oct 99 at 7:53, Lustig, Steven K.. wrote:

[......]
>..  as well as a strip where we
> bond a part subsequently.
[...]
.. just curious - do you mean chip bonding (bare dies), any glue
operations with standard components, or wire bonding?

I'm looking for a reliable process to protect wire bonding areas
(mostly immeesion NiAu for Al wire bonding) with something like a
temporary soldermask against any dirt from SMD process, instead of
expensive cleaning processes like plasma...

Thanks, regards
Matthias Mansfeld


-----------------------------------------------
Matthias Mansfeld Elektronik
* Printed Circuit Board Design and Assembly
Am Langhoelzl 11, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
E-Mail: [log in to unmask]
Internet: http://www.mansfeld-elektronik.de

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2