Gold plating is an extremely demanding process on dry film photoresists;
especially in high dep applications.
There are ways to optimize the process. Give me some details, and perhaps I
can help.
How much Ni/Au are you depositing?
What is the thickness of the dry film?
What are the basic parameters of your gold tank (oz/gal, temp, pH, agitation)?
The type of dry film used can have a big impact on the success/failure of gold
plating process. We sell a couple of products that have excellent resistance
to gold plating. Contact me offline if you would like more information.
Mark Dowding
Regional Technical Service Manager
INSULECTRO
909-943-5758
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|