TECHNET Archives

August 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Tue, 4 Aug 2009 16:24:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Subject:
From:
Steve Kelly <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<D6EC827E1F8C43E0A75A961F5CC298CE@ingemar63eaed8>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (122 lines)
Thanks Inge. Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: August-04-09 2:08 PM
To: [log in to unmask]
Subject: Re: [TN] Wire bond

No problem

/ Inge

----- Original Message ----- 
From: "Steve Kelly" <[log in to unmask]>
To: "'TechNet E-Mail Forum'" <[log in to unmask]>; "'Inge'" 
<[log in to unmask]>
Sent: Tuesday, August 04, 2009 7:55 PM
Subject: RE: [TN] Wire bond


> Hi Inge
> - flex? -  18 micron copper on adhesiveless kapton - stiffener underneath.
> Regards Steve
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
> Sent: August-04-09 1:52 PM
> To: [log in to unmask]
> Subject: Re: [TN] Wire bond
>
> Ceramic : No
> FR-4 : No
> LTCC: No
> Glass: No
> Steel:  No
> Teflon: Yes
>
> /Inge
>
>
> ----- Original Message ----- 
> From: "Steve Kelly" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Tuesday, August 04, 2009 5:36 PM
> Subject: [TN] Wire bond
>
>
> Good Morning,
>
> Does the size of a wire bond pad (in this case with a perfect etch .002
> wide) have any effect on whether the wire bonder does Al wedge or
> Thermosonic gold( I know the gold plating is different) - just asking 
> about
> the process. Thanks. Steve Kelly
>
>
>
> Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)
>
> (416) 750-8433 (work)
>
> (416) 750-0016 (fax)
>
> (416) 577-8433 (cell)
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> ----------------------------------------------------- 
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2