TECHNET Archives

March 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Sun, 1 Mar 2015 22:52:27 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
Thanks Graham . 

I appreciate the reply. 

Rich  Kraszewski 
(920) 969-6075

-----Original Message-----
From: Graham Naisbitt [mailto:[log in to unmask]] 
Sent: Friday, February 27, 2015 8:14 PM
To: IPC TechNet Forum; Richard Kraszewski
Subject: Re: [TN] Required Confromal Coating of Edges of PCB's

Hi Rich,

We missed you in San Diego.

It may very well be that MIL-I-46058 mentions edge coverage, but whether it does or not, keep in mind that there is no solder mask / resist on the card edges. Dependent upon your operating environment, delimitation may be an issue, so coat the edges would be the recommendation.

You might also check IEC 61086, that might have some mention of the issue.

Hope this helps

ATB - Graham N


> On 27 Feb 2015, at 10:51, Richard Kraszewski <[log in to unmask]> wrote:
> 
> Does anyone recall  which  MIL document calls out the requirement to cover  the PCB edges of  assemblies?
> I have been led to believe that one exists but that  more than likely it is not MIL-I-46058C.
> 
> Any thoughts??
> 
> Rich Kraszewski
> Plexus
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2