It is too dangerous to do this (using cyanide).
I think, it would be better to check if the higher thickness of gold plating (on
fingers?) can have an insertion problem. Higher gold thickness does not affect
reliability (solderability), it is good for customer but bad for the supplier
due to price of gold.
If you are trying to remove 1 microns, you can not be sure that the etching is
uniform throughout.
hope it helps
"Y.H. Woo" <[log in to unmask]> on 03/15/2000 07:28:41 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: Jonathan A Noquil/Cebu/Fairchild)
Subject: [TN]
ȸ½Å: [TN] Gold Removal
You could remove extra gold with 1% KCN(Potassium Cyanide) Solution.
It would take about 1 minute to remove 1um gold .
But be careful !!
Hope any help to you.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################